Soldering joins components with melted metal, making a permanent electrical connection. It looks tricky, but good technique is simple: heat the joint, not the solder. Here's everything you need to make clean, reliable joints.
What you need
- A temperature-controlled soldering iron. Cheap irons with no temperature control run too hot or too cold, which makes learning much harder.
- Solder with a flux core. Around 0.7 to 1 mm diameter suits most through-hole work.
- A brass wool tip cleaner or a damp sponge.
- A stand to hold the hot iron safely.
- Flush cutters to trim component legs.
- Ventilation: a fan pulling fumes away, or a fume extractor.
- Safety glasses, because clipped legs and solder can flick.
Leaded or lead-free solder?
| Solder | Melts at | Typical iron temperature |
|---|---|---|
| 63/37 tin-lead | 183 °C | 315 to 370 °C |
| 60/40 tin-lead | 183 to 190 °C | 315 to 370 °C |
| SAC305 lead-free | 217 to 220 °C | 370 to 400 °C |
Leaded solder melts at a lower temperature and flows easily, which makes it forgiving to learn with. Lead-free solder is required in most commercial products sold in the UK and EU, needs a hotter iron, and takes a little more practice. Either is fine for hobby use, as long as you handle leaded solder sensibly: don't eat or drink while soldering, and wash your hands afterwards.
Start with the iron at the lower end of the range and only turn it up if the solder is slow to flow. Too hot burns off the flux and can lift the copper pads off the board.
Making a joint, step by step
- Tin the tip. Melt a little fresh solder onto the hot tip so it's shiny. A shiny tip transfers heat far better than a dull one.
- Place the part through the board and bend the legs slightly so it stays put.
- Heat the joint. Touch the tip so it contacts both the copper pad and the component leg at once. Hold it for a second or two.
- Feed in solder where the leg meets the pad, not onto the iron. The hot joint should melt it and draw it in.
- Remove the solder, then the iron. Use just enough to form a small cone, then take the iron away. The whole thing should take about 2 to 4 seconds.
- Don't move it for a moment while the solder sets.
- Trim the leg just above the joint.
Good joint, bad joint
- Good: a smooth, shiny (or satin, for lead-free) cone that flows onto both the pad and the leg, like a little volcano.
- Cold joint: dull, lumpy or balled up. The joint wasn't hot enough. Reheat it and add a touch of fresh solder.
- Too little: you can see a gap or the hole isn't filled. Reheat and add more.
- Bridge: solder joining two neighbouring pads. Drag the hot tip between them, or remove the excess with solder wick.
After soldering, use a multimeter's continuity mode to check for bridges between power and ground before switching on.
Staying safe
- The tip is hot enough to burn badly. Always return the iron to its stand, and never catch a falling iron.
- The fumes are mostly from the flux and irritate your lungs. Work in a ventilated space and don't lean over the smoke.
- Switch the iron off when you've finished.
Going deeper
Flux: the secret ingredient
Flux removes oxide from metal surfaces so solder can wet them. The flux inside solder wire is usually enough for through-hole work. For surface-mount parts and rework, extra flux (from a pen or syringe) makes a big difference.
- Rosin flux is traditional and forgiving.
- No-clean flux leaves a small residue designed to be safe left on the board.
- Water-soluble flux is very active but must be washed off, as its residue can corrode.
Isopropyl alcohol and a brush clean most flux residue.
Thermal mass
Joints connected to large copper areas, such as ground planes, or big component legs draw heat away fast. Turning the iron up rarely fixes this. Instead, use a larger tip that holds more heat and touches more of the joint. Boards for hand soldering often use "thermal relief" spokes on such pads for this reason.
Surface-mount soldering
- Two-terminal parts (resistors, capacitors): tin one pad, hold the part with tweezers, reflow that pad to tack it down, then solder the other side.
- Chips with many pins: tack two opposite corners, check alignment, add flux, then drag a loaded tip along the row. Clear any bridges with flux and solder wick.
- Hot air and reflow: apply solder paste to the pads, place the parts and heat the whole area with a hot-air tool or reflow oven. This is how parts with pads underneath are soldered.
Desoldering
Solder wick (braided copper) soaks up solder when pressed onto a joint with the iron, and works best with extra flux. A solder sucker removes the solder from through-hole joints in one go. Adding fresh leaded solder to old lead-free joints lowers the melting point and makes removal easier, but don't mix them in work you intend to keep lead-free.
Looking after the tip
Keep the tip tinned when it's hot, especially before switching off or returning it to the stand. Wipe it on brass wool rather than scraping it, never file a plated tip, and lower the temperature or use the iron's sleep mode during breaks, as heat speeds up oxidation.
Sources
The main references behind this guide. Numbers we worked out ourselves, such as the code outputs, come from running the code.